ஜர்னல் ஆஃப் நானோ மெட்டீரியல்ஸ் & மாலிகுலர் நானோடெக்னாலஜி

Photovoltaic Properties and Surface Analysis of Mixed (SnS2)x (CdS)1-x Thin Films by X-ray Photoelectron Spectroscopy (XPS)

MN Amroun*, AH Kacha, K Salim and M Khadraoui

Mixed thin films (SnS2)x(CdS)1-x with various x compositions (x=1, 0.8, 0.2, 0) have been synthesized by spray pyrolysis technique at a substrate temperature of 350°C. Cadmium chloride (CdCl2), Tin chloride (SnCl2), and thiourea (SC(NH2)2) were used as starting chemicals at different compositions. The chemical binding state of the deposited thin films was studied by X-ray photoelectron spectroscopy (XPS). XPS studies indicate the formation of the single phase of CdS and SnS2 thin films and mixed-phase (SnS2)x (CdS)1-x for x=0.8 and x=0.2. Four components of oxygen change in chemical states which are different in BE have been distinguished and studied in the O 1s spectrum. The optical expected absorption capacity and photocurrent (jph) depend on x concentration.

மறுப்பு: இந்த சுருக்கமானது செயற்கை நுண்ணறிவு கருவிகளைப் பயன்படுத்தி மொழிபெயர்க்கப்பட்டது மற்றும் இன்னும் மதிப்பாய்வு செய்யப்படவில்லை அல்லது சரிபார்க்கப்படவில்லை